Matthew Parkinson
Matthew Parkinson
Journeyman Bladesmith (5yr)
Honorable Member
Joined: Feb 15, 2021
Last seen: Apr 18, 2025
Topics: 49 / Replies: 512
Reply
Swords Through The Centuries Iv Swords Of The East Near And Far

yeah that might be helpfull wouldnt it ... editing that now.. thanks Joshua

9 years ago
Reply
Guard Tool

I don't know what this is you are referring to ... but I am intrigued, can you explain? MP

9 years ago
Reply
Fitting A Guard – Topic For September 2016

this is something I struggle with, and as such have been trying to come up with a best practices, to garner more control over it. what have I found...

9 years ago
Reply
Hand Filing (Again)

I dont know how good this is but here you go, sorry it took me so long to get done.

9 years ago
Reply
Brut De Forge Knives – Topic For August 2016

I like taking these to an extreme sometimes, I will forge 98-100% to finished shape with just the edge being cut in after forging and as little filein...

9 years ago
Reply
Hand Filing (Again)

[quote name='Kabe Wolf' date='27 July 2016 - 03:44 PM' timestamp='1469655870' post='17814'] Hey guys, I know this has been covered in the apprentice...

9 years ago
Reply
Metal Cutting Band Saw

we have three band saws in the shop at the moment. two of the cheap smaller 6/9 one set up with a large table in the machine shop and the other set up...

9 years ago
Reply
Pre-Hardening Scratch Size/orientation

I like Ed do AT least 120 pre-heat treat I will also take all of my profile grind lines length wise , nothing crossing the edge. I find this to be alm...

9 years ago
Reply
Filework Tools

I order fromwhen i need new files. I also look around at estate/tag sales for OLD American made files in good shape and buy them if I can. I have been...

9 years ago
Reply
Damascus By Hand

one think to consider, working my hand is especially suited to "viking style" this style is multi bar and all low layer 10-25 seem to look best. the t...

9 years ago
Reply
Help With Blade Finishing

I like the 10x 3m you can get a home depot for under 400 grit and Rhino wet red line for 400 and up. the rhino wet is hands down the BEST paper I have...

9 years ago
Reply
Js Or Ms Failures?

don't discount the help of JS smiths , they have after all passed, and should have a good idea of what is expected. I had Mace look at my knives when ...

9 years ago
Reply
Anybody Use A Magnetic Chuck With A Milling Machine?

millers make things flat and square, surface grinders make things parallel and accurately sized two very different tasks. for this reason they need to...

9 years ago
Reply
Annealing 1095/15N20

do a low temp anneal, at a guess you are getting carbides. For best results harden first then soak at 1150-1200 for half hour or so. most of the time ...

9 years ago
Page 24 / 38