Dagger Design And Grinding

[quote name='Steve Morley' date='28 January 2021 - 01:29 PM' timestamp='1611858572' post='27467'] ... I can't imagine making a dagger that was not b...

4 years ago
Reply
O1 And A2 Uses

Hello Zach, Both of these steels contain carbide forming elements with deep hardening characteristics, making them natural choices for fine slic...

4 years ago
Reply
New Book: Knifemaking Hacks

[quote name='Jason Fry' date='05 December 2020 - 12:36 AM' timestamp='1607146619' post='27248'] I purchased publication rights from Jim Cooper, as w...

4 years ago
Reply
New Book: Knifemaking Hacks

A new book! And I'm in it? Which blade did I send you a picture of, I can't remember?

4 years ago
Reply
Migrating Bevels

Hello Zack, Forge the same angles just keep the very edge thicker, we normally advise around the thickness of a nickel coin. Always remember- t...

4 years ago
Reply
Hello And Spain

Welcome Cristobal.

4 years ago
Reply
Edge Quenching

[quote name='Marc Gelinas' date='06 November 2020 - 10:21 AM' timestamp='1604676100' post='27153'] Keven, Thanks for the info. This is why I jo...

4 years ago
Reply
Edge Quenching

[quote name='Marc Gelinas' date='05 November 2020 - 01:55 PM' timestamp='1604602553' post='27146'] Hello, I am wondering, does the ABS still re...

4 years ago
Reply
Sitting While Grinding

I had the idea of the proper height for years but it took teaching it for many more years to conceptualize it in a way that makes it very clear. You ...

4 years ago
Reply
Sitting While Grinding

I have found that it is possible to do things wrong for so long that it eventually becomes right for you, I am living proof of that. However, there a...

4 years ago
Reply
Banding? From Coffee Treatment

I see plenty of lengthwise banding, I was just sort of ignoring the 45° lines which could be streaks or scratches that appear to be accentuated by th...

4 years ago
Reply
Local Decarburization

Flux is the best answer for any metal outside of the shielding atmosphere. Also, weld zones tend to decarb rather quickly and recarburize, after weld...

4 years ago
Reply
Forged Knife

Nice overall design

4 years ago